Chilled Hard cast iron rolls IV (CCIV) for wire rod mills are rolls made of high-strength, wear-resistant cast iron used for finish and cold rolling in wire rod mills. The hardness of the white layer of the CCIV rollers can reach HS 70-85. It has desirable wear resistance, which can extend the service life of the roller and reduce the frequency of roller replacement. It can withstand impact and vibration under high temperature and high pressure and is not prone to thermal cracks and breakage. It has good dimensional stability and is not easy to deform. It is widely used in various wire rod rolling mills, including high-speed wire rod rolling mills, high-precision wire rod rolling mills, and special steel wire rod rolling mills. Specific applications include: Commonly used in finishing rolling stands of wire rod mills for rolling high-strength, high-precision wire rods. Can withstand shock and vibration at high temperatures of 600-700°C and high pressure.
Hardness HSD: 70-85
Nickel composition %: 3.01-4.5
Suitable for racks: refined and rolled
| Chemical Composition % | ||||||||
|---|---|---|---|---|---|---|---|---|
| Symbol | C | Si | Mn | P | S | Cr | Ni | Mo |
| CCⅢ | 2.90-3.60 | 0.25-0.80 | 0.20-1.00 | ≤0.40 | ≤0.08 | 0.50-1.50 | 2.01-3.00 | 0.20-0.60 |
| CCⅣ | 2.90-3.60 | 0.25-0.80 | 0.20-1.00 | ≤0.40 | ≤0.08 | 0.50-1.70 | 3.01-4.50 | 0.20-0.60 |
| Prosperities & Application | ||||
|---|---|---|---|---|
| Symbol | Hardness | Tensile Strength | Dimension | Application |
| HSD | MPa | MM | ||
| CCⅢ | 65-80 | ≥350 | ¢300-800 | Small section mills, wire mills, hot sheet mills, temper mills. |
| CCⅣ | 70-85 | ≥350 | ||
Wire rod leaves the finishing stands at very high speed and in very small cross-sections, so every micron of roll wear shows up in the product. CCIV addresses this with a hard white chilled layer of 70-85 HSD, supported by a tougher core, and it is positioned among Wire Rod Mill Rolls for the final reduction stages.
Nickel at 3.01-4.5% refines the structure and improves hardenability, supporting a uniform chilled layer and a sound bond with the core. A high-hardness face with a well-supported layer means the roll can hold a fine surface without flaking away.
Small grooves leave no margin for wear. The hardness of the chilled layer keeps the groove profile steady, so rod diameter and roundness stay within tolerance for longer.
At wire rod speeds, rolls experience rapid thermal cycling and vibration. The structure of CCIV absorbs these demands without early surface checking, helping avoid the surface defects that would be copied to the wire.
A hard, smooth groove surface reduces scratches and scale marks, giving a cleaner rod surface for downstream drawing and processing.
Slow, even wear makes roll life forecastable, so changes can be planned with the mill schedule instead of forced by surface failure.
A chilled iron roll costs less than many premium alloy options, while giving the wear life that finishing stands need, keeping cost per ton of wire rod low.
CCIV fits several wire rod production routes, each emphasizing a different strength:
Speed, heat, and vibration define the duty, and the roll's hardness and structural stability are the main assets.
Where diameter tolerance is the selling point, groove stability matters most. CCIV helps hold size within tight limits across a campaign.
Alloy and special steels are harder to roll and demand stronger rolls. The nickel-alloyed chilled layer provides the wear resistance and strength needed for these grades.
CCIV is best placed in the last passes, where wear resistance and surface stability outrank impact tolerance. Positions just ahead of the finishing block with steady loads may also suit it, while Wire Rod Mill Rolls for earlier, heavier stands usually call for a tougher grade.
Hardness level, roll diameter, and groove design should be matched to the rod size range, rolling speed, and cooling arrangement of each line.
It is the outer layer formed by rapid cooling during casting, made of hard carbides in a white iron structure. It provides wear resistance, while the softer core underneath provides strength.
Not typically. Roughing stands face heavy impact and thick stock, which call for tougher grades. CCIV is intended for finishing duty.
Cooling consistency, mill alignment, entry guides, and regrinding practice. Well-maintained conditions let Wire Rod Mill Rolls reach the full campaign length.