Centrifugally cast high chromium iron roll I is a roll made of high chromium iron, produced by a centrifugal casting process. High chromium iron is a very hard material with a hardness of HSD 60-75. The white layer of the centrifugally cast high chromium iron roll has high hardness and wear resistance, which can extend the service life of the roll. It can withstand impact and vibration under high temperatures and high pressure and is not prone to thermal cracks and breakage. Centrifugally cast high-chromium iron roll I have good thermal fatigue resistance and can be used in high-strength, high-precision rolling operations. The centrifugal casting process can make the structure of the roll uniform and dense, thereby improving the dimensional stability of the roll. The centrifugally cast high chromium iron rollers have good dimensional stability and are not easily deformed, ensuring the accuracy and quality of rolled products. With good thermal conductivity, the centrifugal casting process can make the structure of the roll denser and further improve the heat dissipation of the roll. The centrifugally cast high-chromium iron roll I has good heat dissipation, which can reduce the thermal deformation of the roll and improve the quality of the rolled products.
Hardness HSD: 60-75
Nickel composition %: 0.7-1.7
Suitable for racks: refined and rolled
Usage: Hot strip mills, edge roll mills, temper roll mills and medium plate mills; cold strip mills; section universal mill ring.
| Chemical Composition % | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Symbol | C | Si | Mn | P | S | Cr | Ni | Mo | V |
| HCrⅠ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 12.00-15.00 | 0.70-1.70 | 0.70-1.50 | 0.00-0.60 |
| HCrⅡ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 15.01-18.00 | 0.70-1.70 | 0.70-1.50 | 0.00-0.60 |
| HCrⅢ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 18.01-22.00 | 0.70-1.70 | 1.51-3.00 | 0.00-0.60 |
| Prosperities & Application | |||
|---|---|---|---|
| Symbol | Hardness | Tensile Strength | Application |
| HSD | MPa | ||
| HCrⅠ | 60-75 | ≥350 | Hot strip mills, edge roll mills, temper roll mills, and medium plate mills; cold strip mills; section universal mill ring. |
| HCrⅡ | 65-80 | ≥350 | |
| HCrⅢ | 75-90 | ≥350 | |
In centrifugal casting, molten high chromium iron is poured into a rotating mold. Centrifugal force pushes the melt outward against the mold wall and drives impurities toward the inner bore, so the outer layer solidifies dense and clean. For Centrifugally Cast High Chromium Iron Rolls, this process is the foundation for a uniform working layer.
Chromium builds a network of hard carbides in the working layer, which is why high chromium iron is prized for abrasion resistance. HCrI pairs it with nickel at 0.7-1.7% to support matrix hardenability, giving a working hardness of 60-75 HSD that balances wear life against the toughness needed in flat-product service.
A dense, even structure around the full circumference means the roll wears evenly and responds predictably to regrinding.
Fewer internal defects and more consistent hardness around the barrel reduce the risk of local soft spots, which would otherwise cause uneven wear and marks on the strip.
The chromium carbide network resists the sliding contact between roll and strip, so surface finish and profile are kept for more tons.
Heat is carried away from the surface efficiently, so temperature differences stay small and thermal fatigue damage builds slowly. Rolls resist surface cracking and hold their profile through repeated heating and cooling.
Stable roll geometry means stable strip thickness, crown, and flatness, which are the qualities high-precision lines depend on.
Longer service intervals lead to fewer roll changes, less grinding stock lost, and lower roll cost per ton rolled.
HCrI is used where surface quality and wear life determine product value:
In finishing stands, the roll holds a clean surface under high speed and heat. For plate production, a hard, uniform barrel supports thickness control over the full width.
Edge rolls need durability under contact with the strip edge, and temper mills need a surface that stays consistent because it is imprinted directly on the strip.
Cold rolling demands fine surface finish and high hardness. A hard working layer keeps surface roughness stable across a campaign.
In universal section mills, ring-type rolls see complex contact conditions. The dense centrifugal structure supports even wear across the ring's contact surface.
Choice of hardness, size, and finish depends on mill type, stand position, and product requirements. In each of these services, Centrifugally Cast High Chromium Iron Rolls offer a dependable balance of wear life and surface quality.
Spinning the mold promotes a denser, more uniform outer layer with fewer defects, which generally leads to more even wear and better reliability in service.
No. Chilled iron relies on rapid cooling to form hard carbides, while high chromium iron gets its hardness from chromium-rich carbides built into the alloy. HCrI is typically chosen where wear resistance and surface retention are top priorities.
Preheat before rolling, keep cooling even, avoid sudden thermal changes, and regrind on schedule. Well-managed conditions let Centrifugally Cast High Chromium Iron Rolls reach their designed campaign life.