High Chromium Iron Roll II for Tempered Work Rolls is a roll made of high chromium iron that has been subjected to a tempering process. It can improve the organizational structure of the roll, and improve its toughness and impact resistance so that it can withstand greater impact loads and is less likely to break. High chromium iron has good thermal fatigue resistance, can withstand impact and vibration under high temperature and high pressure, and is not prone to thermal cracks and breakage. Quenching and tempering treatment can further improve the thermal fatigue resistance of the roll, making it suitable for high-strength and high-precision rolling operations. Quenching and tempering treatment can eliminate the residual stress of the roll, improve its dimensional stability, make it less likely to deform and ensure the accuracy and quality of rolled products. High chromium iron rolls II for tempered work rolls are also used as finishing work rolls in finishing mills for rolling high-precision steels. High chromium iron rollers II for tempered work rolls are used for rolling stainless steel, heat-resistant steel, and other special steels. High chromium iron roller II used for quenching and tempering work rollers has good impact resistance, and its impact value is generally akv ≥ 15 J/cm2. Higher dimensional accuracy ensures the quality of rolled products.
Hardness HSD: 65-80
Nickel composition %: 0.7-1.7
Suitable for racks: refined and rolled
| Chemical Composition % | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Symbol | C | Si | Mn | P | S | Cr | Ni | Mo | V |
| HCrⅠ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 12.00-15.00 | 0.70-1.70 | 0.70-1.50 | 0.00-0.60 |
| HCrⅡ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 15.01-18.00 | 0.70-1.70 | 0.70-1.50 | 0.00-0.60 |
| HCrⅢ | 2.30-3.30 | 0.30-1.00 | 0.5-1.20 | ≤0.10 | ≤0.05 | 18.01-22.00 | 0.70-1.70 | 1.51-3.00 | 0.00-0.60 |
| Prosperities & Application | |||
|---|---|---|---|
| Symbol | Hardness | Tensile Strength | Application |
| HSD | MPa | ||
| HCrⅠ | 60-75 | ≥350 | Hot strip mills, edge roll mills, temper roll mills, and medium plate mills; cold strip mills; section universal mill ring. |
| HCrⅡ | 65-80 | ≥350 | |
| HCrⅢ | 75-90 | ≥350 | |
High Hardness High Chromium Iron Rolls are known for wear resistance, but hardness alone does not make a good work roll. HCrII adds a quench-and-temper heat treatment after casting, which reshapes the microstructure and rebalances the roll between hardness and toughness.
Hardness remains high at 65-80 HSD, with nickel at 0.7-1.7% contributing to hardenability. What changes is how the roll copes with stress: the matrix is tougher, and the carbide network is better supported, so the surface is less likely to chip or crack when loads spike.
Heat treatment also relieves residual stress locked into the casting. A roll with less internal stress holds its shape better during machining and in service.
Work rolls in finishing stands face bite shocks and strip irregularities. The tempered structure helps absorb these loads, lowering the risk of surface spalling or breakage.
Repeated heating and cooling causes fine cracks over time. A stress-relieved, tempered matrix slows crack initiation and growth, so surfaces stay sound through longer campaigns.
With internal stress reduced, the roll is less prone to distortion between grinding and rolling, and roll geometry remains consistent during the campaign.
A uniform hard surface wears evenly, supporting clean strip surfaces on demanding products.
Planned roll changes replace unplanned ones, and the roll's cost per ton rolled stays competitive for special steel production.
HCrII is aimed at finishing work rolls on lines that handle demanding materials:
Stainless is strong and work-hardens quickly, increasing rolling loads. A tough, hard roll maintains surface quality under these conditions.
These grades are rolled at higher forces and need rolls that resist heat damage and keep gauge accuracy.
Alloy and specialty grades with tight tolerances benefit from consistent roll geometry and wear behavior.
As the last stands set the final thickness and surface, a stable, wear-resistant roll face is a direct contributor to product quality.
Hardness within 65-80 HSD should be chosen according to material, stand position, and rolling speed. For this duty, High Hardness High Chromium Iron Rolls with proper heat treatment give mills a more forgiving option than untreated rolls.
Quenching builds hardness, and tempering relieves stress and improves toughness. Together they give a better balance of wear resistance and resistance to cracking and shock.
Tempering may slightly lower peak hardness compared with an untreated roll, but 65-80 HSD remains well within the high-hardness range, and the gain in toughness usually justifies the trade.
Choose HCrII for work rolls that see impact, hard-to-roll materials, or a risk of thermal cracking. Choose a harder grade where loads are steady and surface retention is the top priority. High Hardness High Chromium Iron Rolls cover both needs, but the right choice depends on stand duty.