High Nickel Infinitely Chilled Cast Iron Roll IV is a high-performance roll designed to meet the demanding rolling requirements of modern steel mills. Made of high nickel-chromium-molybdenum alloy, it has extremely high hardness and wear resistance and can withstand heavy loads and high-intensity wear environments. Its hardness can reach HRC 70-83, which is 2-3 times that of ordinary cast iron rolls, which can significantly reduce the frequency of roll replacement and maintenance costs. It has thermal crack resistance, which can avoid thermal cracks at high temperatures and extend its service life. It has anti-adhesion properties, which can reduce the adhesion of steel billets to the roll surface, reduce surface roughness, and improve the quality of rolled products. It has good peeling resistance, which can prevent the roller surface from peeling and extend its service life. The high-nickel infinitely chilled cast iron roll IV is a high-performance, high-reliability roll that can significantly increase roll service life, improve rolled product quality, reduce rolling costs, and improve production efficiency. It is an ideal choice for modern steel mills to improve production efficiency and product quality.
Hardness HSD: 70-83
Nickel composition %: 3.01-4.8
Suitable for racks: refined and rolled
Usage: Plate mills, temper mills, hot strip mills.
High Nickel Cast Iron Mill Rolls
| Chemical Composition % | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Symbol | C | Si | Mn | P | S | Cr | Ni | Mo | V | W | Nb |
| ICⅡ | 2.90-3.60 | 0.60-1.2 | 0.40-1.20 | ≤0.25 | ≤0.08 | 0.70-1.20 | 1.01-2.00 | 0.20-0.60 | |||
| ICⅢ | 2.90-3.60 | 0.60-1.2 | 0.40-1.20 | ≤0.25 | ≤0.08 | 0.70-1.20 | 2.01-3.00 | 0.20-1.00 | |||
| ICⅣ | 2.90-3.60 | 0.60-1.5 | 0.40-1.20 | ≤0.10 | ≤0.05 | 1.00-2.00 | 3.01-4.80 | 0.20-1.00 | |||
| ICⅤ | 2.90-3.60 | 0.60-1.5 | 0.40-1.20 | ≤0.10 | ≤0.05 | 1.00-2.00 | 3.01-4.80 | 0.20-2.00 | 0.20-2.00 | 0.00-2.00 | 0.00-2.00 |
| Prosperities & Application | |||
|---|---|---|---|
| Symbol | Hardness | Tensile Strength | Application |
| HSD | MPa | ||
| ICⅡ | 55-72 | ≥160 | Plate mills, temper mills, hot strip mills. |
| ICⅢ | 65-78 | ≥350 | |
| ICⅣ | 70-83 | ≥350 | |
| ICⅤ | 77-85 | ≥350 | |
ICIV sits at the top of the infinite chill range. Nickel at 3.01-4.8% is combined with chromium and molybdenum to produce a hard, stable working layer that resists wear while keeping its hardness deep below the surface. Chromium forms hard carbides, molybdenum strengthens the matrix and its stability at temperature, and nickel promotes a uniform structure through the barrel.
Working hardness reaches 70-83 HSD, a level aimed at finishing duty. At this hardness, the surface can keep a polished finish through long campaigns, which is why High Nickel Cast Iron Mill Rolls of this kind are chosen for positions where product appearance counts as much as dimension.
Because the chill is infinite, hardness declines gradually rather than ending at a thin shell, so regrinding between campaigns keeps exposing useful working metal.
Strip and plate buyers judge product by its surface. A hard, dense roll face wears evenly and resists roughening, which limits the marks passed to the steel and keeps finish consistent over a long run.
Hot steel can pick up on roll surfaces, leaving defects on the product. The carbide-rich surface helps limit this adhesion, so the roll stays cleaner and requires less intervention.
Thermal cycling and rolling pressure can lead to surface flaking or crack networks. A stable alloyed matrix and graded structure help the roll withstand these stresses, reducing the chance of an early, unplanned change.
Slow wear means rolled tonnage per campaign is easier to forecast, and fewer roll changes keep mill schedules steady.
Better surface and stable profile cut rejects and rework, while longer life lowers roll cost per ton. For mills producing high-value flat products, those savings often outweigh the premium of the alloy.
ICIV is aimed at flat-product lines where finish and flatness are critical:
In finishing stands, the roll meets high speed, heat, and tight thickness and surface requirements. Wear resistance and surface integrity are the priority, and ICIV supplies both.
Wide barrels carry heavy loads across the full width. A hard, uniform working layer keeps the roll profile consistent so plate thickness and flatness remain under control.
Temper rolling imparts final surface character to strip. Here a durable, smooth roll face matters most, since any change in the roll surface appears directly on the product.
Barrel size, hardness level, and surface finish requirements should be specified according to mill type, stand position, and product grade. Hardness in the 70-83 HSD range can be matched to the severity of duty. For these demanding positions, High Nickel Cast Iron Mill Rolls such as ICIV give mills a way to protect surface quality over long campaigns.
Chromium adds hard carbides for wear resistance, and molybdenum improves matrix strength and stability at temperature. Nickel supports a uniform structure, so the three work as a system instead of single additions.
Greater hardness can reduce toughness, so ICIV is intended for finishing positions where loads are steadier and shock is limited. Stands with heavy impact are better served by lower-hardness, tougher grades.